Akasel A/S
No products in the cart.
Polycrystalline diamond spray for metallographic sample preparation.
Aka-Spray Poly leaves a free-cutting layer of diamonds resulting in high removal rates.
Diamond concentration of 26.5 ct/l 100% polycrystalline diamonds Median (50%) 0.71 µm Tolerance 0.65 – 0.77 µm Upper limit (99%) 1.3 µm
Shake before use, this product is not stable.
165 ml