Polycrystalline diamond spray for metallographic sample preparation.
Aka-Spray Poly leaves a free-cutting layer of diamonds resulting in high removal rates.
Diamond concentration of 26.5 ct/l 100% polycrystalline diamonds Median (50%) 5.7 µm Tolerance 5.42 – 5.98 µm Upper limit (99%) 7.9 µm
Shake before use, this product is not stable.
165 ml