Polycrystalline diamond spray for metallographic sample preparation.
Aka-Spray Poly leaves a free-cutting layer of diamonds resulting in high removal rates.
Diamond concentration of 26.5 ct/l 100% polycrystalline diamonds
Median (50%) 9.6 µm Tolerance 9.12 – 10.08 µm Upper limit (99%) 12.9 µm
Shake before use, this product is not stable.
165 ml